Industrial Coatings

Why Do Industrial Coatings Fail?

Industrial coatings are used to solve a wide range of engineering problems, from reducing friction and wear to providing chemical resistance, corrosion protection, release properties and electrical insulation.

But even a coating with excellent technical properties can fail if it is not correctly selected, applied or used.

Peeling, blistering, cracking, excessive wear, discolouration and loss of adhesion are all signs that something has gone wrong. The cause isn't always the coating itself. In many cases, coating failure results from a combination of surface preparation, application, substrate, operating conditions and material selection.

Understanding why coatings fail is therefore an important part of specifying the right coating system.

Table of Contents

What Causes Industrial Coating Failure?

Industrial Coating Troubleshooting: Symptoms, Causes and Checks

How Can Industrial Coating Failures be Prevented?

Coating Failure is often a System Problem

What Causes Industrial Coating Failure?

A coating needs to be considered as part of the complete engineering system. The coating, substrate and operating environment all interact. Common causes for failure include:

1. Poor Surface Preparation

One of the most common causes of coating failure is inadequate preparation of the substrate.

Before a coating is applied, the surface may need to be cleaned, degreased, blasted, chemically treated or otherwise prepared to provide the required surface condition.

Contamination such as:

  • Oil and grease
  • Dust
  • Oxides
  • Rust
  • Previous coatings
  • Moisture
  • Processing residues

can interfere with adhesion.

Even a coating with excellent inherent adhesion can fail if it is applied to a contaminated or unsuitable surface.

Why does this cause peeling?

A coating needs to form a reliable bond with the substrate.

If contaminants sit between the coating and substrate, the coating may initially appear satisfactory but eventually lift, blister or peel when exposed to heat, chemicals, mechanical stress or moisture.

Good coating performance starts before the coating is applied.

2. Choosing the Wrong Coating

There is no single industrial coating that is ideal for every application.

Different coating chemistries provide different combinations of:

  • Friction reduction
  • Release
  • Chemical resistance
  • Temperature resistance
  • Corrosion protection
  • Wear resistance
  • Surface hardness
  • Electrical properties
  • Purity

For example, a PTFE coating may be selected where low friction and release properties are important.

A PFA coating may be more appropriate where chemical resistance and high-purity performance are required.

FEP coating can provide useful release and chemical-resistant properties, while ETFE and ECTFE can be considered where greater toughness or corrosion resistance is required.

Ceramic coating systems can provide a different combination of hardness, durability and temperature performance.

Selecting a coating based on one property alone can therefore result in failure elsewhere.

3. The Coating is Too Thick

More coating does not necessarily mean better protection.

Every coating system has an appropriate thickness range. If a coating is applied too thickly, it can create problems such as:

  • Cracking
  • Poor curing
  • Internal stresses
  • Uneven surfaces
  • Dimensional changes
  • Reduced adhesion

This can be particularly important for precision components where coating thickness affects clearances, fits or surface geometry.

4. The Coating is Too Thin

The opposite problem can occur when insufficient coating is applied.

A coating that is too thin may not provide the required:

  • Chemical resistance
  • Wear resistance
  • Corrosion protection
  • Release performance
  • Surface coverage

Thin areas can also expose the substrate prematurely, particularly on edges, corners and complex geometries.

Uniform coverage is therefore just as important as the nominal coating thickness.

5. Incorrect Curing

Many industrial coating systems require controlled curing or baking to achieve their intended properties.

If the temperature, time or process conditions are incorrect, the coating may not develop the expected performance.

Potential consequences include:

  • Poor adhesion
  • Reduced mechanical strength
  • Incomplete curing
  • Cracking
  • Blistering
  • Reduced chemical resistance
  • Premature wear

The curing process needs to be appropriate for both the coating and the substrate, particularly where the substrate is sensitive to elevated temperatures.

6. Chemical Attack

A coating can be exposed to chemicals throughout its service life, including:

  • Acids
  • Alkalis
  • Solvents
  • Oils
  • Fuels
  • Process chemicals
  • Cleaning agents

A coating that is resistant to one chemical may not be resistant to another, particularly at elevated temperatures or concentrations.

Chemical compatibility should therefore be assessed against the actual process media and operating conditions, rather than relying on a general statement such as “chemically resistant”.

For aggressive chemical environments, fluoropolymer coatings such as PTFE, PFA, FEP or ECTFE may be considered depending on the application.

7. Excessive Temperature

Every coating has a temperature range within which it is designed to perform.

Operating outside that range can accelerate:

  • Degradation
  • Loss of mechanical properties
  • Oxidation
  • Discolouration
  • Cracking
  • Adhesion loss

However, maximum temperature should not be considered in isolation. A coating exposed to high temperature while simultaneously subjected to chemicals, pressure, abrasion or mechanical loading may behave very differently from the same coating under temperature alone.

8. Mechanical Damage

Even a correctly specified coating can be damaged by mechanical forces.

Examples include:

  • Impact
  • Scratching
  • Abrasion
  • Sharp edges
  • Poor handling
  • Excessive contact pressure
  • Repeated sliding

Once the coating has been damaged, the exposed substrate may become vulnerable to corrosion, chemical attack or further wear.

Where abrasion or mechanical contact is expected, the coating should therefore be selected for its wear performance as well as its primary function.

9. Thermal Expansion Differences

The coating and substrate do not necessarily expand and contract at the same rate when temperature changes.

Repeated heating and cooling can therefore create stresses at the coating/substrate interface.

Over time, this can contribute to:

  • Cracking
  • Delamination
  • Blistering
  • Loss of adhesion

This is particularly important where components experience significant temperature cycling.

10. The Substrate isn't Suitable

A coating cannot compensate for every limitation of the underlying component.

The substrate can affect:

  • Adhesion
  • Thermal behaviour
  • Corrosion resistance
  • Surface preparation
  • Maximum processing temperature
  • Dimensional stability

The same coating system may therefore behave differently on stainless steel, aluminium, carbon steel or another substrate.

The substrate should form part of the coating specification from the beginning of the selection process.

11. The Application Process isn't Appropriate

Different coating systems require different application techniques, including:

The application method affects coating uniformity, thickness, coverage and finish.

Complex components can also present challenges around internal surfaces, recesses, sharp corners and difficult-to-access areas.

12. The Service Conditions Have Changed

Sometimes a coating fails because the application has changed after the original specification.

For example, a component may originally have operated at a lower temperature, pressure, cycle rate, chemical concentration or contact load.

A change in any of these conditions can affect coating life.

If equipment is upgraded or a process is modified, the original coating specification should be reviewed rather than assuming the existing system will continue to perform in the same way.

Industrial Coating Troubleshooting: Symptoms, Causes and Checks

If a coating has already failed, the appearance of the failure can provide useful clues about what went wrong.

What you see Possible causes What to check
Peeling or flaking Poor adhesion, contamination, inadequate surface preparation, incorrect curing Substrate preparation, cleanliness, surface profile, curing conditions and coating system
Blistering or bubbling Trapped moisture or contamination, excessive film thickness, chemical attack, poor curing Substrate condition, moisture, coating thickness, curing process and service chemicals
Cracking Excessive coating thickness, thermal cycling, substrate movement, over-temperature exposure Coating thickness, temperature range, substrate movement and curing
Delamination Poor adhesion, incompatible coating/substrate, contamination, thermal or mechanical stress Adhesion, substrate material, preparation method and operating conditions
Rapid wear Incorrect coating selection, excessive load, abrasion, unsuitable mating surface Contact pressure, sliding speed, counterface, wear mechanism and coating specification
Discolouration Excessive temperature, chemical exposure, UV or process contamination Operating temperature, chemicals, environmental exposure and coating chemistry
Pinholes or exposed areas Insufficient coating thickness, poor application, difficult geometry Film thickness, application technique, component geometry and coverage
Loss of release/non-stick performance Surface damage, contamination, wear, incorrect coating selection Surface condition, cleaning process, temperature and mechanical contact
Corrosion beneath the coating Coating damage, poor adhesion, inadequate coverage or substrate preparation Coating integrity, substrate condition, edges, joints and exposed areas
Dimensional problems Excessive coating thickness or uneven application Coating thickness, tolerances, masking and application process

These symptoms are not definitive diagnoses. Several failure mechanisms can produce similar symptoms, so the coating, substrate and service conditions should be assessed together before deciding on corrective action.

How Can Industrial Coating Failures be Prevented?

Preventing coating failure starts with understanding the complete operating environment and selecting the coating system accordingly.

Before specifying a coating, consider:

  • Operating temperature and temperature cycling
  • Chemical exposure and concentration
  • Pressure and contact loads
  • Friction and wear
  • Required service life
  • Substrate material
  • Surface preparation requirements
  • Required coating thickness
  • Application and curing method
  • Dimensional tolerances
  • Purity or regulatory requirements

The coating should then be selected around the combination of requirements.

Primary requirement Potential coating approach
Low friction PTFE and other low-friction fluoropolymer coatings
Release / non-stick PTFE, FEP and other suitable fluoropolymer systems
Chemical resistance PTFE, PFA, FEP, ECTFE and other suitable systems
High purity PFA and other appropriate high-purity systems
Corrosion protection ECTFE, ETFE and other application-specific systems
Hardness / durability Ceramic coating systems
Multiple requirements Application-specific or multi-layer coating systems

These are starting points rather than universal recommendations. The appropriate coating depends on the complete combination of substrate, operating conditions and required performance.

Once the coating has been selected, surface preparation, application, thickness control and curing need to be controlled to the coating specification.

Coating Failure is often a System Problem

When an industrial coating fails, it is tempting to look at the coating material first.

But the cause may be elsewhere.

The problem could be:

  • The wrong coating for the chemical environment
  • Poor surface preparation
  • Incorrect coating thickness
  • Inadequate curing
  • A substrate issue
  • Excessive temperature
  • Mechanical damage
  • Unexpected changes in service conditions

This is why successful industrial coating requires more than simply applying a layer of material to a component.

The coating, substrate, manufacturing process and operating environment all need to work together.

Need Help Selecting an Industrial Coating?

Fluorocarbon combines materials expertise, coating technology, component manufacturing and engineering support to help customers select and apply coatings for demanding industrial applications.

Our coating capabilities include fluoropolymer and ceramic systems for applications requiring low friction, release, chemical resistance, corrosion protection, wear resistance and other specialised surface properties.

If a coating is failing, or you are specifying a coating for a new application, our engineering team can help assess the substrate, service conditions, coating requirements and manufacturing process to identify an appropriate solution.

Contact Us